Escorene AES Ultra UL 7741 物性表

Escorene AES Ultra UL 7741 物性表
物理性能额定值
单位制
测试方法
熔流率 (190°C/2.16 kg)
43
g/10 min
ASTM D1238
醋酸乙烯含量
26.7
wt%
ExxonMobil Method


Escorene AES Ultra UL 7741详情见附件

需要了解Escorene AES Ultra UL 7741 更多详情,赵先生:13424755533或QQ: 27660005